Polymer Property : Tensile Strength = 4300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 29.6 MPa
4300 psi
ASTM D638, ASTM D1708
ScanTube THV Tubing
Information provided by ScanTube, Inc.
Tensile Strength 29.6 MPa
4300 psi
2 in/min; ASTM D638
Braskem TR3120C Random Copolymer Polypropylene
Description: Superior color and processing stability, low odor, good flow and set-up behavior, excellent see through clarity.Applications: Suggested uses include housewares, reusable food containers..
Tensile Strength 29.6 MPa
4300 psi
Cross; IPC TM-650 2.4.18.3
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards
Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist..
Tensile Strength 29.6 MPa
4300 psi
ASTM D638
Americas Styrenics STYRON® 478 High Impact Polystyrene
Product CharacteristicsGood glossExcellent balance of flow and stiffnessFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsAppliancesMedicalHousewaresConsumer electronicsIn..
Tensile Strength 29.6 MPa
4300 psi
2 in/min; ASTM D638
Braskem TI4900M Impact Copolymer Polypropylene
Description: Very high flexural modulus.Applications: Suggested uses include compounding, automotive interior trim, intricately designed parts, thin walled parts.Process: Injection Molding.This resi..