Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 16.0 MPa | >= 2320 psi | Type IV, 500mm/min; ASTM D638 |
S&E Specialty Polymers SE900-5 PVC Description: PVC weatherable, integral colored, filledApplications: Roof Ditch Molding Core which meets the Ford WSKM4D689-A4Information provided by S&E Specialty Polymers |
|||
Tensile Strength | 16.0 MPa | 2320 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Tensile Strength | 16.0 MPa | 2320 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Tensile Strength | 16.0 MPa | 2320 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio.. |
|||
Tensile Strength | 16.0 MPa | 2320 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Tensile Strength | >= 16.0 MPa | >= 2320 psi | DIN 53504 |
NEXA® PFX9010 Perfluoroelastomer NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi.. |
|||
Tensile Strength | 16.0 MPa | 2320 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data) TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl.. |
|||
Tensile Strength | 16.0 MPa | 2320 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Tensile Strength | 16.0 MPa | 2320 psi | ASTM D2095 |
Permabond UV620 UV-curable Adhesive PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I.. |
|||
Tensile Strength | 16.0 MPa | 2320 psi | ISO 37 |
Kraton® D4271 J (O/E SBS) Branched Block Copolymer Description: Kraton D4271 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene of 45% mass. It is supplied from Japan in the physical forms identified in .. |
|||
Tensile Strength | 16.0 MPa | 2320 psi | Average; ASTM D412 Method A |
Seals Eastern 5794 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Strength | 16.0 MPa | 2320 psi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-A885 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Tensile Strength | 16.0 MPa @Strain 100 % |
2320 psi @Strain 100 % |
ISO 37 |
BASF Elastollan B 60 D TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tensile Strength | >= 16.0 MPa | >= 2320 psi | ISO 37 |
Austin Novel Materials Texalan® 365A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Strength | 16.0 MPa @Strain 100 % |
2320 psi @Strain 100 % |
ISO 37 |
BASF Elastollan S 98 A TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tensile Strength | >= 16.0 MPa | >= 2320 psi | ISO 37 |
Austin Novel Materials Texalan® 665A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |