Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 101 MPa | 14600 psi | DIN EN ISO 527 |
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan.. |