Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 8.85 MPa @Treatment Temp. 140 °C, Time 3.629e+6 sec |
1280 psi @Treatment Temp. 284 °F, Time 1008 hour |
heat aging; ASTM D573-99 |
Multibase TPSiV® 3111-70A Thermoplastic Elastomer TPSiV™ material for injection molding and extrusion applicationsAPPLICATIONS: Solution for appliance, sports and leisure, and construction applications where excellent hydrolysis resistance, high a.. |
|||
Tensile Strength | 8.80 MPa | 1280 psi | ISO 37 |
Multibase TPSiV® 4000-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob.. |
|||
Tensile Strength | 8.83 MPa @Strain 100 % |
1280 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible B8501 Polyvinyl Chloride, Flexible (PVC, Flexible) A flexible Vinyl compound for hose and tubing applications with enhanced physical characteristics.Information provided by PolyOne |
|||
Tensile Strength | >= 8.83 MPa | >= 1280 psi | ASTM D 638 |
Karina E CAK 75-48/1 Black PVC Compound Reclaimed PVC compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 8.83 MPa | >= 1280 psi | ASTM D 638 |
Karina 653D10/1-C-IS White PVC Compound Anti fungus PVC compound for extrusion/drain blow molding.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 8.83 MPa | >= 1280 psi | ASTM D 638 |
Karina 75/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 8.83 MPa | >= 1280 psi | ASTM D 638 |
Karina 75/202 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 8.83 MPa | >= 1280 psi | ASTM D 638 |
Karina CAK 75-48/1 Black PVC Compound Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 8.83 MPa | >= 1280 psi | ASTM D 638 |
Karina 760-48/1-E-AC-LF Black PVC Compound Flame retardant and lead and cadmium free PVC compound recommended for extrusion and injection of parts for general purposes.Information provided by Karina Indústria e Comércio de Plásticos.. |
|||
Tensile Strength | 8.80 MPa | 1280 psi | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-30A/B Elastomer KE-1950-30 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |