Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 84.0 MPa | 12200 psi | at Yield; ISO 527-1/-2 |
Quadrant EPP Nylatron® MC901 PA 6, blue, cast (ISO Data) This modified cast nylon 6 grade with its distinctive blue colour exhibits higher toughness, flexibility and fatigue resistance than Ertalon 6 PLA. It has proved to be an excellent material for gear.. |
|||
Tensile Strength | 84.3 MPa | 12200 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BFM30-EL04B2 Nylon 6 30% Mineral Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 84.0 MPa | 12200 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK) AvaSpire® AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. .. |
|||
Tensile Strength | 84.1 MPa | 12200 psi | ASTM D638 |
Ensinger Tecapeek® XP-106 Compression Molded PEEK Compound, 40% Fiberglass Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Tensile Strength | 84.0 MPa | 12200 psi | 50 mm/min; ASTM D638 |
Solvay Specialty Polymers AvaSpire® AV-621 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 is an unreinforced polyaryletherketone (PAEK) that offers improved ductility and impact strength relative to PEEK while retaining most of the key performance attributes of PEEK. The .. |
|||
Tensile Strength | 84.0 MPa | 12200 psi | 5 mm/min; ISO 527-1 |
Sax Polymers SAXALEN PPH327G28 Polypropylene Homopolymer, 28% Glass Filled SAXALEN PPH327G28 is a 28% glass filled Polypropylene - Homopolymer injection molding grade with increased stiffness.Information provided by SAX Polymers |