Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 78.5 MPa | 11400 psi | ASTM D638 |
Samyang Trirex® 3025GN10 Polycarbonate, Reinforced Flame Retardancy PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3025GN10 is a reinforced flame retardant grade.Applications: LCD Panel Frame (dimensio.. |
|||
Tensile Strength | 78.5 MPa | 11400 psi | ASTM D638 |
Gromax CCP PBT 6730-104F Glass/Mineral Filled Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w.. |