Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 60.0 - 90.0 MPa | 8700 - 13100 psi | Compression; ISO 527 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Injection; ISO 527 |
Raschig Group DECAL® 666/8/2B Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meets the allowe.. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on .. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Injection and Compression; ISO 527 |
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
Tensile Strength | 50.0 - 90.0 MPa | 7250 - 13100 psi | Injection; ISO 527 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Compression; ISO 527 |
Raschig Group DECAL® 152CL Phenolic Glass-fiber and mineral reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This product meet.. |
|||
Tensile Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Compression; ISO 527 |
Raschig Group RESINOL® 400 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |