Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 62.0 - 69.0 MPa | 8990 - 10000 psi | specimen type 1, 5 mm/mn; ASTM D638 |
Lucite International XL Sanitary Ware Acrylic Sheet Lucite® XL continuous-cast cross-linked acrylic sheet is specially formulated for deep-draw thermoforming. It is used primarily for production of spas.Benefits: Smooth surface; Infinite colors an.. |