Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 4.48 MPa | 650 psi | ASTM D412 |
S&E Specialty Polymers GTPR-1358A Thermoplastic Rubber material designed for winter boot applications requiring excellent abrasion and stitch tear. Available in a wide range of colors.Information provided by S&E Specialty Polymer.. |
|||
Tensile Strength | >= 4.48 MPa | >= 650 psi | ASTM D412 |
Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tensile Strength | >= 4.48 MPa | >= 650 psi | ASTM D412 |
Parker Chomerics Tecknit SC-Consil® FR862 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tensile Strength | 4.48 MPa @Strain 100 % |
650 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible D75M0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tensile Strength | 4.48 MPa | 650 psi | |
Teknor Apex Tekbond® TB 2007 Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | 4.48 MPa | 650 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4945A Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Tensile Strength | 4.48 MPa | 650 psi | ASTM D412 |
Teknor Apex Telcar® OBC 4945F Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Tensile Strength | 4.48 MPa | 650 psi | Silicone Property; ASTM D412 |
Arlon 49442R0075 0.0075" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassThis data represents typical values for the production material and should not be used as material specifications.I.. |
|||
Tensile Strength | 4.48 MPa | 650 psi | Compound Property; ASTM D412 |
Arlon 49442R0075EP 0.0075" (0.190 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Substrate: Style 1681 FiberglassSide 2: Acrylic PSAThis data Represents typical values for the production material. The data should not be used to w.. |
|||
Tensile Strength | 4.48 MPa | 650 psi | Silicone Property; ASTM D412 |
Arlon R36338R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Uncured Silicone Rubber Substrate: Style 7628 FiberglassSide 2: Cured Silicone RubberAppearan.. |
|||
Tensile Strength | 4.48 MPa | 650 psi | Silicone Property; ASTM D412 |
Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 8 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Prim.. |
|||
Tensile Strength | 4.48 MPa | 650 psi | Silicone Property; ASTM D412 |
Arlon Thermabond® T20 (99710W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 15 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Pri.. |
|||
Tensile Strength | >= 4.48 MPa | >= 650 psi | Compound Property |
Arlon CP-339R Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Tensile Strength | >= 4.48 MPa | >= 650 psi | ASTM D412 |
Parker Chomerics CHO-SEAL® S6600 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Molded onlyRoHS CompliantInformation provided by Chomerics |
|||
Tensile Strength | >= 4.48 MPa | >= 650 psi | ASTM D412 |
Parker Chomerics Tecknit SC-Consil® 861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |