Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D638 |
Quadrant EPP TIVAR® 88-2 UHMW-PE, Premium Lubricant Filled Lining Material (ASTM Product Data Sheet) Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic f.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D638 |
Quadrant EPP TIVAR® CERAM P UHMW-PE, Premium Microsphere Filled (ASTM Product Data Sheet) |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D638 |
Quadrant EPP TIVAR® Dockguard - UHMW-PE - Black UV Stabilized UHMW-PE (ASTM Product Data Sheet) |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D412 |
Northstar Polymers MSS-A95BQ Ester Base High Performance Polyurethane This high-performance quasi-polyester system is one of a family of polymer systems developed by Northstar Polymers for demanding work environments. Urethane elastomers molded with this system exhib.. |
|||
Tensile Strength | 37.9 MPa @Thickness 3.17 mm |
5500 psi @Thickness 0.125 in |
ASTM D638 |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength | 37.9 MPa @Thickness 3.17 mm |
5500 psi @Thickness 0.125 in |
ASTM D638 |
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant Contains UV absorber.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength | 37.9 - 41.4 MPa | 5500 - 6000 psi | ASTM D638 |
Mar-Bal MB3000-15 Thermoset Polyester Composite Molding Compound A superior chemical resistant material with excellent flame and track resistance.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D638 |
Techmer ES Elastoblend® PBT IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D638 |
Techmer ES Luriblend® TPX-PPO/HIPS-02072 BK Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Lubricated, Good Wear Resistance, Low Friction and HomopolymerUL File Number: E157318Information provided by TP Composites,.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D412 |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio.. |
|||
Tensile Strength | 37.9 MPa @Temperature 75.0 °C, Time 0.000 sec |
5500 psi @Temperature 167 °F, Time 0.000 hour |
Immersion in Water |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D638 |
Ecomass® 1080ZD92 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | 2 in/min; ASTM D638 |
Braskem CP350WV Homopolymer Polypropylene Description: Narrow Molecular Weight Distribution, Antistatic, NucleatedApplications: Suggested Uses Include Fast Cycle Injection Molding, Large-Part Injection Molding, Disposable DrinkwareThis resi.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | 2 in/min; ASTM D638 |
Braskem FF450WV Homopolymer Polypropylene Description: Excellent Processability, Nucleated.Applications: Suggested Uses Include Fast-Cycle Injection Molding and CompoundingProcess: Injection Molding.This resin meets the requirements for ole.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | 2 in/min; ASTM D638 |
Braskem FPT350WV3 Homopolymer Polypropylene Description: Narrow molecular weight distribution, antistatic, nucleated, very good mold release.Applications: Suggested uses include fast-cycle injection molding, large-part injection molding, disp.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | 2 in/min; ASTM D638 |
Braskem FT021N Homopolymer Polypropylene Description: Contact clarity, nucleated, high flexural modulus. Applications: Suggested uses include thermoforming, portion-controlled packaging, deli containers. Process: Thermoforming. This resi.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | 2 in/min; ASTM D638 |
Braskem ZS-751 Homopolymer Polypropylene Description: Superior stiffness, good static charge dissipation, excellent mold release, nucleated.Applications: Suggested uses include closures, overcaps, cosmetic packaging, disposable cutlery.Pro.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D638 |
Aaron Industries AVPP C 200-2 Virgin Polypropylene Melt flow index may be specified. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D638 |
Aaron Industries AVPS GP(crystal) 100-1 Virgin Polystyrene - Crystal Melt flow index may be specified. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D412/D638 |
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane Features: It has the highest heat resistance of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and b.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | ASTM D412 |
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Eur.. |
|||
Tensile Strength | 37.9 - 51.7 MPa | 5500 - 7500 psi | |
Bulk Molding Compounds BMC T15(GPS) General Purpose Molding Compound BMC T15(GPS) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPS) is well suited for injection, transfer or compression.. |
|||
Tensile Strength | 37.9 - 51.7 MPa | 5500 - 7500 psi | |
Bulk Molding Compounds BMC T15(GPT) General Purpose Molding Compound BMC T15(GPT) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GPT) is well suited for injection, transfer or compression.. |
|||
Tensile Strength | 37.9 MPa | 5500 psi | 2 in/min; ASTM D638 |
Braskem FF650WV Homopolymer Polypropylene Description: Excellent processability, nucleated.Applications: Suggested uses include fast-cycle injection molding and compounding.Process: Injection Molding.This resin meets the requirements for ol.. |