Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 35.2 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 35.2 MPa
5100 psi
ASTM D638
Quadrant EPP TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet)
Tensile Strength 35.2 MPa
5100 psi
2 in/min; ASTM D638
Braskem 52T30V Homopolymer Polypropylene
Description: Clarified, Excellent Mold Release, Excellent Flow CharacteristicsApplications: Suggested Uses Include Housewares, Storage Boxes, Containers, VialsInformation provided by Braskem
Tensile Strength 35.2 MPa
5100 psi
2 in/min; ASTM D638
Braskem D180M Homopolymer Polypropylene
Description: Low Gas FadeApplications: Suggested Uses Include BCF Multi-Filaments, High Tenacity Continuous Filament Yarn, Fine Denier Staple FibersThis resin meets the requirements for olefin polym..
Tensile Strength 35.2 MPa
5100 psi
2 in/min; ASTM D638
Braskem FT021NH Homopolymer Polypropylene
Description: High Clarity, Improved AppearanceApplications: Suggested Uses Include Thermoforming, Drink Cups, Deli ContainersThis resin meets the requirements for olefin polymers as defined in 21 CF..
Tensile Strength 35.2 MPa
5100 psi
ASTM D638
Aaron Industries AAROLENE® ARPP C 200-2 Polypropylene Compounded Resin
AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified.
Tensile Strength 35.2 MPa
5100 psi
2 in/min; ASTM D638
Braskem D180A2 Homopolymer Polypropylene
Description: Excellent Melt StabilityApplications: Suggested Uses Include Caps and Closures, Housewares, BCF Multi-Filaments, High Tenacity Continuous Filament Yarn, Fine Denier Staple FibersThis re..
Tensile Strength 35.2 MPa
5100 psi
Machine; IPC TM-650 2.4.18.3
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards
Only Woven Glass Reinforced PTFE/Ceramic with Dk of 10.2 or greaterHigh Copper Peel Strength allows for thinner etched line widthsLowest insertion loss availableLarger Panel sizes availableLow moist..
Tensile Strength 35.2 MPa
5100 psi
ASTM D638
Americas Styrenics STYRON® 649D High Heat Crystal Polystyrene
Product CharacteristicsExcellent moldabilityExcellent gloss in coextrusionExcellent clarityFood Contact CompliantTypical ApplicationsDisposable cutleryHousewaresCompact disc and DVD jewel boxesDesk ..
Tensile Strength 35.2 MPa
5100 psi
ASTM D638
Aaron Industries AAROLENE® ARPS HI-100-4 Polystyrene Compounded Resin
AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified.
Tensile Strength 35.2 MPa
5100 psi
ASTM D638
Quadrant EPP Sanalite® PP, Homopolymer Polypropylene Cutting Board (FDA, USDA, & NSF) (ASTM Product Data Sheet)
Copyright © lookpolymers.com All Rights Reserved