Polymer Property : Tensile Strength = 24.8 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 24.8 MPa
3600 psi
ASTM D638
Quadrant EPP TIVAR® 88 W/BurnGuard, Flame Retardant Lining Material (ASTM Product Data Sheet)
Promotes reliable, steady bulk material flow Abrasion-, chemical- and corrosion-resistant Low coefficient of friction No moisture absorption Reduces or eliminates arching, ratholing and erractic fl..
Tensile Strength 24.8 MPa
3600 psi
ASTM D412
Northstar Polymers MPG-D70A Room-Temperature-Curable Polyurethane Casting Elastomer
MPG-D70A is room-temperature-curable polyurethane casting elastomer system designed for molding polyurethane parts with tough, but flexible physical characteristics. The typical applications for th..
Tensile Strength 24.8 MPa
3600 psi
ASTM D638
I. Stern HIPS 8 High Impact Polystyrene Injection Grade
Features:Good processing characteristicsComplies with FDA requirements as described in Title 21 CFR 177.1640ApplicationsDisplaysHouse waresStructural FoamInformation provided by I. Stern & Co. Inc.
Tensile Strength 24.8 MPa
3600 psi
Lucite International Elvacite ® 2045 Acrylic Resin
Elvacite® 2045 is a high molecular weight iso-butyl methacrylate polymer. Elvacite® 2045 is useful in topcoats for vacuum metallized plastics and in lacquers for other solvent – sensitive..
Tensile Strength 24.8 MPa
3600 psi
2 in/min; ASTM D638
Braskem TI4130G Impact Copolymer Polypropylene
Description: Medium izod impact, good blush resistance, good low temperature drop impact.Applications: Suggested uses include furniture, housewares, automotive interior trim. UL temperature index of..
Tensile Strength 24.8 MPa
3600 psi
ASTM D638
Americas Styrenics STYRON® 487R High Impact Polystyrene
Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliancesPackaging/disposablesHousewaresInformation provided by Amer..