Polymer Property : Tensile Strength = 19.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina SDB 35/3-LMP Ivory PVC Compound
Heavy metal free PVC compound, recommended for insulation of automotive wires.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 19.6 MPa
>= 2840 psi
NBR NM-IEC 60811-1-1
Karina SDB 40/1-HSF Ivory PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength 19.6 MPa
2840 psi
ISO 527
Gromax 1140LH TPE
Product Description: 1140LH is Low modulus grade with nominal Durometer hardness of 40D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like inject..
Tensile Strength >= 19.6 MPa
>= 2840 psi
35 min cured; ASTM D412
Iran Petrochemical (PCC) SBR-1712 Styrene Butadiene Rubber
SBR–1712 is staining type cold SBR ,extended with 27.5 part of highly aromatic oil. Provided that the compounds are formulated and processed correctly, the vulcanized SBR–1712 has very g..
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina 920D32/91 Orange PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina 924D10/349-IS White PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina E 105440-35/1-Y-IS-SD-LM Ivory PVC Compound
Heavy metal free PVC compound, recommended for thin wall insulation of automotive electrical wires for working at the temperature range of -40°C to 105°CInformation provided by Karina Indús..
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina E 57/200-D-AT-IS-SD Clear PVC Compound
PVC compound recommended for shrink films.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina E 670D48/1-CY-IS-SD Black PVC Compound
PVC compound with elevated insulation resistance.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina E 701D02/128-SD Yellow PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina 57/200-D-AT-IS-SD Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina E 57/201-D-IS-SD Compound PVC Crystal
Clear/crystal PVC compound specially developed for skin films.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina E 85/209-D-AT-IS-SI Clear PVC Compound
Compound recommended for stretch films.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A7020 TPU for Ink
Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen..
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A7710 TPU for Ink
Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen..
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A7810H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A8000F Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A8361E Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A8510H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A8511H TPU for Ink
Thermoplastic polyurethane elastomer for inkAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen printing, and spray applicati..
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A8550 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A9080 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength 19.6 MPa
2840 psi
Taiwan Sheen Soon Sheenthane® A9612K Film Grade Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for blown filmInformation provided by Taiwan Sheen Soon Co., LTD.
Tensile Strength >= 19.6 MPa
>= 2840 psi
ASTM D 638
Karina E 57/200-D-AT-IS-SI-SD Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.