Mechanical Properties Metric English Comments
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina TR-607D48/1-Y-IS-BZ Black PVC Compound
Heavy metal free PVC compound additivated with nitrile rubber.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina TR-607D48/1-Y-IS-BZ Black PVC Compound
Heavy metal free PVC compound additivated with nitrile rubber.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 700-48/1-B-IS-BZ. Black PVC Compound
Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 72/204-D-AT-H Crystal PVC Compound
Nontoxic PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 75/204-D-AT-IS-H Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 800-DA-10/1-A-AT-IS White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 804D40/146-AT Green PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 809D10/161-BY-IS White PVC Compound
PVC compound recommended for extrusion of forniture profile and flexible laminated.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 900D06/366-B-IS-BZ Blue PVC Compound
Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 901D10/146-B-AT White PVC Compound
Non toxic PVC compound recommended for injection of parts for general applications.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina E 70/236-DA-IS Clear PVC Compound
PVC compound recommended for freezer hanging screens extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina E 70/236-D-IS Clear PVC Compound
PVC compound recommended for freezer hanging screens extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina E 75/236-D-IS Clear PVC Compound
PVC compound recommended for extrusion of butcher's shop curtain.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina E 75/244-D-AT-IS-SI Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina E 800D10/7-A-IS White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 740-DA-18/339-A-IS-BZ Gray PVC Compound
Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Karina 800D10/7-A-IS White PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.