Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 0.689 MPa | >= 100 psi | ASTM D3574-75 Test E |
Rogers Corporation Poron® Shock Seal™ 4790-79-20 Urethane Foam, Industrial Grade Thickness: 0.062"- 0.188"Color: BlackInformation provided by Rogers Corporation. |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | ASTM D412 |
Parker Chomerics Tecknit Consil®-II 841 Molded Silver-Filled Silicone Elastomer Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi.. |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | ASTM D412 |
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation.. |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | ASTM D412 |
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by .. |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | ASTM D412 |
Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer Description: Consil-V is an extruded silicone elastomer filled with silver-plated inert particles. The V-shape cross section is ideally suited for applications requiring low closure force gasketing... |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ C41NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tensile Strength | 0.689 MPa | 100 psi | Die A; ASTM D412 |
Monmouth Rubber & Plastics Durafoamâ„¢ C43 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK2121 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK3131 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | |
Monmouth Rubber & Plastics Durafoamâ„¢ N231XS 100% Neoprene Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | Compound Property, Side 2 |
Arlon R35121R063 0.063" (1.60 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material speci.. |
|||
Tensile Strength | >= 0.689 MPa | >= 100 psi | Compound Property |
Arlon 51976R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Tensile Strength | 0.689 MPa | 100 psi | Silicone Property; ASTM D412 |
Arlon 48360X005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassFlame Resistance: Product meets Title 14 CFR 25.856(a) Appendix F, Part VI (amdt. 25-111).. |