Polymer Property : Tear Strength, Total = 0.899 lb (f) Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength, Total 4.00 N
0.899 lb (f)
MD; ISO 6383/2
Borealis Himod™ FT6273 LDPE for Film
Himod FT6273 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Tear Strength, Total 4.00 N
0.899 lb (f)
MD; ISO 6383/2
Borealis Himod™ FT6274 LDPE for Film
Himod FT6274 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Tear Strength, Total 4.00 N
0.899 lb (f)
MD; ISO 6383/2
Borealis Himod™ FT7293 LDPE for Film
Himod FT7293 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Tear Strength, Total 4.00 N
0.899 lb (f)
MD; ISO 6383/2
Borealis Himod™ FT7294 LDPE for Film
Himod FT7294 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Tear Strength, Total 4.00 N
0.899 lb (f)
MD; ISO 6383/2
Borealis Himod™ FT7324 . LDPE for Film
Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Tear Strength, Total 4.00 N
0.899 lb (f)
Initial in TD; ASTM D1004
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..