Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength, Total | 1.20 N | 0.270 lb (f) | M.D., Elmendorf; ASTM D1922 |
Eastman Eastman Embrace Copolyester for Shrink Film Applications:Flexible packagingIV containersLabels to fit high contour containersShrink packagingWrap around designKey Attributes:Excellent clarityExcellent printabilityGood chemical resistanceGood .. |