Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0021 - 0.0055 cm/cm

@Time 86400 sec
0.0021 - 0.0055 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Verton WV007XXP PBT (Europe-Africa-Middle East)
LNP VERTON* WV007XXP is a compound based on Polybutylene Terephalate resin containing Long Glass.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.