Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0389 cm/cm

@Time 86400 sec
0.0389 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP 2X03624H FP-F (FEP)
LNP* THERMOCOMP* 2X03624H is a compound based on FEP resin containing Proprietary Filler(s).