Polymer Property : Linear Mold Shrinkage, Flow = 0.0072 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0072 cm/cm

@Time 86400 sec
0.0072 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6
LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Linear Mold Shrinkage, Flow 0.0072 cm/cm

@Time 86400 sec
0.0072 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Asia Pacific)
LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Linear Mold Shrinkage, Flow 0.0072 cm/cm

@Time 86400 sec
0.0072 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP KONDUIT PTF2BXXX PA 6 (Europe-Africa-Middle East)
LNP KONDUIT* PTF2BXXX is a compound based on Nylon 6 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Linear Mold Shrinkage, Flow 0.0072 cm/cm

@Time 86400 sec
0.0072 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP EX03599H PEI
LNP* LUBRICOMP* EX03599H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant.
Linear Mold Shrinkage, Flow 0.0072 cm/cm

@Time 86400 sec
0.0072 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP
LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized.