Physical Properties Metric English Comments
Density 1.10 - 1.20 g/cc

@Temperature 25.0 °C
0.0397 - 0.0434 lb/in³

@Temperature 77.0 °F
RTM 120 bisphenol epoxy resin containing reactive diluent; ISO 1675
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System
RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process.
Density 1.10 g/cc

@Temperature 43.3 °C
0.0397 lb/in³

@Temperature 110 °F
BASF Pluracol® 1158 Specialty Polyol
Description: Pluracol® 1158 polyol is a polyol which can be used in a wide variety of applications. It can be employed as a cross-linking agent for rigid foam as well as coatings and elastomers. Wh..
Density 1.10 g/cc

@Temperature 60.0 °C
0.0397 lb/in³

@Temperature 140 °F
BASF Pluracol® SG-470 Rigid Polyol
Description: Pluracol® SG-470 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent ..
Density 1.10 g/cc

@Temperature 25.0 °C
0.0397 lb/in³

@Temperature 77.0 °F
Liquid
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems
Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing..
Density 1.10 g/cc

@Temperature 60.0 °C
0.0397 lb/in³

@Temperature 140 °F
BASF Pluracol® 735 Rigid Polyol
Description: Pluracol® 735 polyol is a modifying polyol which can be used in a wide variety of rigid foam applications and can be formulated using crude MDI, crude TDI, or TDI quasi-prepolymers. Fo..
Density 1.10 g/cc

@Temperature 60.0 °C
0.0397 lb/in³

@Temperature 140 °F
BASF Pluracol® SG-450 Rigid Polyol
Description: Pluracol® SG-450 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent ..