Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.997 g/cc @Temperature 50.0 °C |
0.0360 lb/in³ @Temperature 122 °F |
Concentration 0.01 kg FeCl3/kg |
Solvay Chemicals Ferric chloride Ferric chloride is a red brown aqueous solution, with a slight odor.EINECS: 231-729-4/CAS: 7705-08-0/UN: 2582Information provided by Solvay |
|||
Density | 0.997 g/cc @Temperature 40.0 °C |
0.0360 lb/in³ @Temperature 104 °F |
Concentration 0.01 kg HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (2 wt% - 10 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |
|||
Density | 0.997 g/cc @Temperature 48.9 °C |
0.0360 lb/in³ @Temperature 120 °F |
|
BASF Pluracol® 1026 Molded Foam Polyol Description: Pluracol® 1026 polyol is a high molecular weight triol developed for the manufacture of high resiliency molded foams. HR foams made with Pluracol 1026 in combination with graft polyols.. |