Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.948 - 0.955 g/cc @Temperature 23.0 °C |
0.0342 - 0.0345 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT21-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |
|||
Density | 0.948 - 0.955 g/cc @Temperature 23.0 °C |
0.0342 - 0.0345 lb/in³ @Temperature 73.4 °F |
|
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |