Physical Properties | Metric | English | Comments |
---|---|---|---|
Volatile Organic Compounds (VOC) Content | 144 - 840 g/l | 144 - 840 g/l | Average value: 527 g/l Grade Count:32 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Volatile Organic Compounds (VOC) Content | 144 g/l | 144 g/l | |
Blue River Coatings High Performance Acrylic Sanding Sealer BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC SANDING SEALER is a waterbased wood sealer to fill the grain. The product is designed to be a sandable self-sealing topcoat for wood. HIGH PERFORMANCE AC.. |
|||
Volatile Organic Compounds (VOC) Content | 144 g/l | 144 g/l | |
Blue River Coatings High Performance Acrylic Topcoat BLUE RIVER COATINGS HIGH PERFORMANCE ACRYLIC TOPCOAT is a water dispersible acrylic enamel. HIGH PERFORMANCE ACRYLIC TOPCOAT is designed to be a low VOC and EPA compliant coating with excellent cove.. |
|||
Volatile Organic Compounds (VOC) Content | 144 g/l | 144 g/l | |
Blue River Coatings Low VOC Primer Sealer BLUE RIVER COATINGS LOW VOC PRIMER SEALER is a high quality, single component primer. Performance obtained is equal or superior to that of single component solvent primers. LOW VOC PRIMER SEALER off.. |
|||
Volatile Organic Compounds (VOC) Content | 144 g/l | 144 g/l | |
Blue River Coatings Primer Sealer-PSWP BLUE RIVER COATINGS PRIMER SEALER-PSWP is a high quality, single component primer formulated specifically for priming wood, vinyl, and most plastic substrates. Performance obtained is equal or super.. |