Polymer Property : Storage Temperature = 80.6 °F Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Storage Temperature <= 27.0 °C
<= 80.6 °F
Permabond QFS10 Cyanoacrylate Activator
The PERMABOND QFS 10 accelerates the cure of cyanoacrylate adhesives to provide a shorter set time. It can be used in a variety of applications but is especially useful when bonding porous or poorly..
Storage Temperature <= 27.0 °C
<= 80.6 °F
Permabond QFS16 Cyanoacrylate Activator
The PERMABOND QFS 16 accelerates the cure of cyanoacrylate adhesives to provide a shorter set time. It can be used in a variety of applications but is especially useful when bonding porous or poorly..
Storage Temperature <= 27.0 °C
<= 80.6 °F
Permabond Nitroethane Solvent for Cyanoacrylate
The PERMABOND SOLVENT is extremely effective for dissolving cyanoacrylate bonds or removing cured excess adhesive. It is not recommended for use on acrylic plastics. The solvent base is Nitroethane...
Storage Temperature <= 27.0 °C
<= 80.6 °F
3 months
ACC QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting
QSil 940 is a special purpose, two-component condensation cure siloxane elastomer that exhibits excellent release properties unless a primer is used which results in excellent adhesion. The material..
Storage Temperature <= 27.0 °C
<= 80.6 °F
Clean and Dry
3M Dyneon™ FX 5929 Polymer Processing Additive
Information provided by the Dyneon division of 3M.