Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS Reinforced PC/ABS with high stiffness and low CTE. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 300 °C |
24 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific) Reinforced PC/ABS with high stiffness and low CTE. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 1008/0001 Polyvinylidene Fluoride
(discontinued **) Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Melt Index of Compound | 24 g/10 min @Load 2.16 kg, Temperature 280 °C |
24 g/10 min @Load 4.76 lb, Temperature 536 °F |
|
Honeywell Aegis™ CSD High Barrier Nylon
(discontinued **) Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw.. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 280 °C |
24 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 280 °C |
24 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 280 °C |
24 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 250 °C |
24 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 11008/0001 Polyvinylidene Fluoride PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing, wire and cable, semiconductor, and oil and gas industries. PVDF is also gaining rec.. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 11008/0003 Polyvinylidene Fluoride PVDF is ideal for multiple applications across a wide array of industries. Widely used in the chemical processing, wire and cable, semiconductor, and oil and gas industries, PVDF is also gaining rec.. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 6108/0001 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |
|||
Melt Index of Compound | 24 g/10 min @Load 5.00 kg, Temperature 230 °C |
24 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 6008/0001 Polyvinylidene Fluoride Polyvinylidene Fluoride (PVDF) is ideal for multiple applications across a wide array of industries. Widely used in the chemical process industry, wire and cable industry, semiconductor industry, an.. |