Polymer Property : Moisture Vapor Transmission = 0.356 cc-mil/100 in²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.140 cc-mm/m²-24hr-atm
0.356 cc-mil/100 in²-24hr-atm
ASTM F1249
Chevron Phillips HiD® 9650 HDPE Blown Film Resin  (discontinued **)
Resin Type: Linear Polyethylene CopolymerCharacteristics: Copolymerization Enhances Film Toughness, Excellent Film Drawdown, Unique Molecular Architecture Gives Moisture Barrier Properties Typical o..
Moisture Vapor Transmission 0.140 cc-mm/m²-24hr-atm
0.356 cc-mil/100 in²-24hr-atm
Proc. E; ASTM E96
DuPont Teijin Films Mylar® OB12AF Polyester Packaging Film, 50 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OB12AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the op..
Moisture Vapor Transmission 0.140 cc-mm/m²-24hr-atm
0.356 cc-mil/100 in²-24hr-atm
Proc. E; ASTM E96
DuPont Teijin Films Mylar® OB12 Polyester Packaging Film, 50 Gauge
Data provided by DuPont Packaging Polymers.Mylar® OB12 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer and polyvinylidene chloride (PVDC) layer on the oppo..