Physical Properties | Metric | English | Comments |
---|---|---|---|
Moisture Vapor Transmission | 0.860 cc-mm/m²-24hr-atm | 2.18 cc-mil/100 in²-24hr-atm | ASTM E96 |
DuPont™ Tedlar® TWH20BS3 Satin White Polyvinyl Fluoride Film Properties of DuPont™ Tedlar® polyvinyl fluoride (PVF) biaxially oriented film include excellent resistance to weathering, outstanding mechanical properties, and inertness towards a wide variety o.. |
|||
Moisture Vapor Transmission | 0.860 cc-mm/m²-24hr-atm | 2.18 cc-mil/100 in²-24hr-atm | Proc. E; ASTM E96 |
DuPont Teijin Films Mylar® OL13 Polyester Packaging Film, 50 Gauge Data provided by DuPont Packaging Polymers.Mylar® OL13 (formerly known as XM110) is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat seal.. |