Polymer Property : Moisture Vapor Transmission = 0.100 cc-mm/m²-24hr-atm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Moisture Vapor Transmission 0.100 cc-mm/m²-24hr-atm
0.254 cc-mil/100 in²-24hr-atm
ASTM F1249
Chevron Phillips HiD® 9662 HDPE Blown Film Resin  (discontinued **)
Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give..
Moisture Vapor Transmission 0.100 cc-mm/m²-24hr-atm
0.254 cc-mil/100 in²-24hr-atm
ASTM F1249
Chevron Phillips MarFlex® 9659 HDPE Blown Film Resin
Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give..
Moisture Vapor Transmission 0.100 cc-mm/m²-24hr-atm
0.254 cc-mil/100 in²-24hr-atm
ASTM E96 Procedure E
DuPont Teijin Films Mylar® M33 Polyester Film, 50 Gauge, PVDC Coated
Data provided by DuPont Packaging Polymers.A transparent polyester packaging film, solvent coated on both sides with a PVDC copolymer. the coating is heat sealable, and is an excellent moisture and..