Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 129 cm³/g | 129 cm³/g | Reduced viscosity, K value = 71; ISO 1628-2 |
SolVin 271DF Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized and semi-rigid profiles and pipes
- blowing of plasticized films
Calendering : opaque or transparent, plasticized and semi-r.. |
|||
Viscosity Test | 129 cm³/g | 129 cm³/g | Reduced viscosity, K value = 71; ISO 1628-2 |
SolVin 271GA Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized and semi-rigid pipes for medical applications
- plasticized film for blood bags
Injection molding : plasticized and semi-rig.. |
|||
Viscosity Test | 129 cm³/g | 129 cm³/g | Reduced viscosity, K value = 71; ISO 1628-2 |
SolVin 271PC Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized and semi-rigid profiles and pipes
- blowing of plasticized films
Calendering : opaque or transparent, plasticized and semi-r.. |
|||
Viscosity Test | 129 cm³/g | 129 cm³/g | Viscosity Number |
DSM Akulon® F223-D (Dry) Low/Medium Viscosity Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Viscosity Test | 129 cm³/g | 129 cm³/g | Viscosity Number; ISO 307, 1157, 1628 |
DSM Akulon® F-X9183 PA6 Low/Medium Viscosity |