Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity Test | 91 cm³/g | 91 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® T 7331 POS151 000000 PBT + PET, 30% Glass Fiber
(discontinued **) PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Viscosity Test | 91 cm³/g | 91 cm³/g | Viscosity number; ISO 307, 1157, 1628 |
Lanxess Pocan® T 7331 000000 PBT + PET, 30% Glass Fiber PBT+PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Viscosity Test | 91 cm³/g | 91 cm³/g | Viscosity number; ISO 1628-5 |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |