Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 33.0 - 54.0 dynes/cm | 33.0 - 54.0 dynes/cm | Average value: 41.6 dynes/cm Grade Count:5 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |