Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 500 - 1800 cP | 500 - 1800 cP | #2/20 rpm |
Mallard Creek Polymers ROVENE® 6101 Styrene-Acrylic Emulsion ROVENE® 6101 is a stiff, non-film forming high-gloss extending vehicle for flexographic and gravure inks and overprint varnishes. It is intended for use primarily on paper and paperboard.APPLICAT.. |
|||
Brookfield Viscosity | 500 - 1800 cP | 500 - 1800 cP | #20/200 |
Mallard Creek Polymers Rovene® 6103 Resin Supported Emulsion Rovene® 6103 is a soft, film forming vehicle that provides good water and rub resistance for flexographic and gravure inks and overprint varnishes. Rovene® 6103 can be used as the film forming.. |
|||
Brookfield Viscosity | 400 - 1800 cP | 400 - 1800 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Emulsion 34935 Anionic paraffin/ethylene acrylic acid wax emulsion Description: Anionic paraffin/ethylene acrylic acid wax emulsionUsage: Michem® Emulsion 34935 is best used as an additive where excellent water beading properties are required It is primarily use.. |
|||
Brookfield Viscosity | 1200 - 1800 cP @Temperature 25.0 °C |
1200 - 1800 cP @Temperature 77.0 °F |
20% Toluene solution; BAM 922 |
Kraton® G1657 M (SEBS) Linear Block Copolymer Description: Kraton G1657 M is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form id.. |
|||
Brookfield Viscosity | 1400 - 1800 cP | 1400 - 1800 cP | Brookfield RVF sp 4, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 46-10/16 Polyester based TPU Pearlstick 46-10/16 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a high thermoplasticity level. Solubility: .. |
|||
Brookfield Viscosity | 1400 - 1800 cP | 1400 - 1800 cP | Brookfield RVF sp 4, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 45-80/16 Polycaprolactone based TPU Pearlstick 45-80/16 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a very low crystalliz.. |
|||
Brookfield Viscosity | 1200 - 1800 cP | 1200 - 1800 cP | 1% in 1% KCl, LVT, 60 rpm, spindle 3; TI-1110 |
Solvay RHODICARE D Surfactant Description: Rhodicare® D is an anionic bio-polymer with excellent stabilizing, thickening and suspending properties. It has high electrolyte stability over a wide range of pH and fast hydration .. |
|||
Brookfield Viscosity | 200 - 1800 cP | 200 - 1800 cP | 1% sol. in 1% KCl Brookfield LV 60 rpm spindle n°3; TI-1110 |
Solvay RHODOPOL® 23 Surfactant Description: Rhodopol® 23 is Standard grade Xanthan Gum. It exhibits high pseudoplastic behavior and rapid hydration rate. This grade is registered on the FALCON list of approved substances.Ident.. |
|||
Brookfield Viscosity | 1200 - 1800 cP | 1200 - 1800 cP | 1% sol. in 1% KCl Brookfield LV 60 rpm spindle n°3; TI-1110 |
Solvay RHODOPOL® T Surfactant Description: Transparent grade xanthan gum. It is It exhibits high pseudoplastic behavior effective thickening and stabilizing agent.Identification: XANTHAN GUMCAS: 11138 – 66 – 2Available.. |
|||
Brookfield Viscosity | 1400 - 1800 cP @Temperature 25.0 °C |
1400 - 1800 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 201 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 201: Polyester resin.. |
|||
Brookfield Viscosity | 1200 - 1800 cP | 1200 - 1800 cP | 1% in 1% KCl, LVT, 60 rpm, spindle 3; TI-1110 |
Solvay RHODICARE H Surfactant Description: Rhodicare® H is an anionic bio-polymer with excellent stabilizing, thickening and suspending properties. It has high electrolyte stability over a wide range of pH and fast hydration ra.. |