Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 90000 - 110000 cP @Temperature 25.0 °C |
90000 - 110000 cP @Temperature 77.0 °F |
RVT, Spindle #7 @ 20rpm |
Lord Adhesives Metech 3270 Silver Conductor This composition is a silver bearing paste designed for screen print application of a fired conductive electrode. It forms a highly adherent bond to many compositions including alumina. The paste ha.. |