Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | <= 450 cP | <= 450 cP | Spindle # 2, rpm 60 |
Michelman® Michem® Emulsion 80939M Nonionic paraffin wax emulsion Description: Nonionic paraffin wax emulsionUsage: Michem® Emulsion 80939M provides excellent water resistance when used as an additive for Industrial coatings.We serve many markets through Michem.. |
|||
Brookfield Viscosity | 450 - 750 cP | 450 - 750 cP | Brookfield RVF sp 3, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 45-90/06 Polycaprolactone based TPU Pearlstick 45-90/06 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a low crystallization.. |
|||
Brookfield Viscosity | 450 - 750 cP | 450 - 750 cP | Brookfield RVF sp 3, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); ISO 2781 |
Lubrizol Advanced Materials Pearlstick® 45-90/12 Polycaprolactone based TPU Pearlstick 45-90/06 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a small amount of anti-adherent in the formulation. It has a low crystallization.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Hydrafine® 90W Clay Hydrafine® 90W is a premium quality, high brightness, fine particle size clay. Excellent for use in high brightness coated printing paper and board – providing a superb balance of print glo.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Hydrafine® Clay Hydrafine® is fine particle size coating clay used extensively for high quality coated paper and board. Industry: PAPER & PACKAGINGUses: Coated 1S Label, Coated Bleached Board, Coated, Recycle Bo.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Hydragloss® 90 Clay Hydragloss® 90 is a high brightness, fine glossing, coating clay used in heavy weight coated paper and coated board application. Its fine particle size and excellent flow properties allow for hi.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Hydragloss® Clay Hydragloss® is a medium brightness, fine glossing, coating clay used in heavy weight coated paper and coated board application. Its fine particle size and excellent flow properties allow for hig.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Hydraprint® Kaolin Clay - Filler Hydraprint® kaolin clay is a standard delaminated filler for paper applications. Industry: PAPER & PACKAGINGUses: Coated 1S Label, Coated Bleached Board, Coated Recycled Board, Coated Natural Kra.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Hydrasperse® Kaolin Clay - Filler Hydrasperse® is a #2 coating clay available in standard and high brightness. Can be used over a wide range of coating applications.Industry: PAPER & PACKAGINGUses: Coated 1S Label, Coated Bleache.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin KaMin® 80B Kaolin Clay - Waterwashed KaMin® 80B is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appl.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin KaMin® 95 Kaolin Clay - Waterwashed KaMin® 95 is a medium-brightness, kaolin clay filler for paints, adhesives and related industries. It has a neutral pH, is acid-resistant and environmentally friendly.Industry: Adhesives & Sealan.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin KaMin® HG Kaolin Clay - Waterwashed KaMin® HG is an economical, general purpose, water-washed kaolin with fine particle size and intermediate brightness. It is suitable for water borne paint, ink and adhesive applications.Industry:.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Omnifil® Kaolin Clay - Filler Omnifil® kaolin clay is a standard brightness fine fraction filler for paper applications.Industry: PAPER & PACKAGINGUses: Coated Recycled Board, Coated Natural Kraft, LinerboardInformation provi.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Polyfil® XB Kaolin Clay - Waterwashed Cost effective, kaolin extender offering improved consistency vs air floated clays, spray-dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, EPDM, Wire & CableIn.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Polyplate® P Kaolin Clay - Delaminated Polyplate® P is a high brightness, delaminated clay intended for use in latex paints, water flexography inks, water-based adhesives or water-based systems where increased hiding, tinting strength.. |
|||
Brookfield Viscosity | 450 cP | 450 cP | ASTM D2196, LVT, Spindle #2 @ 30rpm |
Lord Adhesives Chemglaze® V209 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Brookfield Viscosity | 450 cP | 450 cP | ASTM D2196, LVT, Spindle #2 @ 30rpm |
Lord Adhesives Chemglaze® V300 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Polyfil® DL Kaolin Clay - Delaminated Large, platy delaminated clay that reduces gas/vapor permeability, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, MasterBatchInform.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Polyfil® FB Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® FB offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® FB is a moderate brightness wate.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Polyfil® HG Kaolin Clay - Waterwashed Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline .. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
20 RPM |
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |
|||
Brookfield Viscosity | 450 cP @Temperature 125 °C |
450 cP @Temperature 257 °F |
|
Westlake Epolene® N-34 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-34 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Brookfield Viscosity | 450 cP @Temperature 125 °C |
450 cP @Temperature 257 °F |
|
Westlake Epolene® N-34P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-34P is a polyethylene (PE) homopolymer powder that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Brookfield Viscosity | 450 cP @Temperature 25.0 °C |
450 cP @Temperature 77.0 °F |
|
Loctite® 3341 Light Cure Acrylic Adhesive Medical Grade BondersLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant products are designe.. |
|||
Brookfield Viscosity | 450 cP @Temperature 160 °C |
450 cP @Temperature 320 °F |
ETM E-31 |
ExxonMobil ESCOREZ™ 2173 (Europe) Petroleum Hydrocarbon Resin ESCOREZ™ 2173 is a narrow molecular weight aromatic modified aliphatic resin giving excellent compatibility with natural and most synthetic rubbers and with EVA copolymers. It provides low viscosit.. |
|||
Brookfield Viscosity | 450 - 650 cP | 450 - 650 cP | RVF #3 sp @ 20 rpm @ 25°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Brookfield Viscosity | 450 cP | 450 cP | Part B |
BCC Products DP-11-90 Urethane Casting DP-11-90 is an unfilled, low viscosity, quick setting two component urethane system. An easy to use 1 to 1 mix ratio (Part A/Part B), DP-11-90 offers the user a 3 minute working time with parts demo.. |
|||
Brookfield Viscosity | 450 - 700 cP | 450 - 700 cP | RVF #2 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 10 Neoprene Contact Adhesive 3M™ Scotch-Weld™ Neoprene Contact Adhesive 10 is a multi-purpose contact adhesive which may be used to bond plastic laminate, aluminum, steel, wallboard, wood, masonry, rubber and canvas.Informati.. |
|||
Brookfield Viscosity | 450 - 1250 cP | 450 - 1250 cP | RVF #3 sp @ 20 rpm @ 27°C |
3M Scotch-Weld™ 1870 Industrial Adhesive Features: A fast drying, highly flexible adhesive with very long tack range and good water resistanceFor bonding fabrics and most other lightweight materials with little or no tendency to stain or b.. |
|||
Brookfield Viscosity | 450 - 750 cP | 450 - 750 cP | Brookfield RVF sp 2, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 46-10/06 Polyester based TPU Pearlstick® 46-10/06 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a high thermoplasticity level. Solubility: .. |