Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 1000 - 1400 cP | 1000 - 1400 cP | Brookfield RVF sp 3, 20 rpm, Solution 15% MEK (MQSA Nº 55 A); MQSA 40A |
Lubrizol Advanced Materials Pearlstick® 46-10/12 Polyester based TPU Pearlstick 46-10/12 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a high thermoplasticity level. Solubility:.. |
|||
Brookfield Viscosity | 1000 - 1400 cP @Temperature 25.0 °C |
1000 - 1400 cP @Temperature 77.0 °F |
|
C.O.I.M. EXTER S® S 203 Special Laminate Description: The Exter S product line contains a large number of unsaturated polyester resin products with an array of properties and applications.Specific Notes for ESTER S® S 203: Polyester resin.. |