Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | <= 900 cP | <= 900 cP | #2/20 rpm |
Mallard Creek Polymers BarrierPro® 4550 SBR Emulsion BARRIER PRO® 4550 is an anionic carboxylated styrene-butadiene copolymer latex containing a non-staining antioxidant. Features: highly stable, good compatibility with fillers and pigments, etc., .. |
|||
Brookfield Viscosity | <= 900 cP | <= 900 cP | #20/200 |
Mallard Creek Polymers Rovene® 4045 Styrene-Butadiene Emulsion Description: Rovene® 4045 is recommended in applications where soil and aggregate stabilization and binding are required. Rovene® 4045 can be used in the process of road construction, landscap.. |
|||
Brookfield Viscosity | <= 900 cP | <= 900 cP | Spindle # 3, rpm 60 |
Michelman® Michem® Lube 135 Anionic paraffin/polyethylene wax emulsion Description: Anionic paraffin/polyethylene wax emulsionUsage: Michem® Lube 135 promotes water and mar resistance and anti-blocking properties when used as an additive in various coating formulati.. |
|||
Brookfield Viscosity | 900 - 1500 cP | 900 - 1500 cP | Measured on 25% mass solution in toluene at 25°C; KM 06 |
Kraton® D1102 B (SBS) Liner Block Copolymer Description: Kraton D1102 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 29.5%. It is supplied from South America in the physical form identifie.. |
|||
Brookfield Viscosity | 900 cP @Temperature 25.0 °C |
900 cP @Temperature 77.0 °F |
Toluene solution. Neat polymer concentration, 25%w. |
Kraton® D1112P (SIS) Linear Block Copolymer (SIS) styrene-isoprene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact q.. |
|||
Brookfield Viscosity | 900 cP | 900 cP | RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in THF |
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin .. |
|||
Brookfield Viscosity | 900 - 1500 cP | 900 - 1500 cP | RVF #2 sp @ 20 rpm @ 80°F |
3M Scotch-Weld™ 2141 Neoprene Rubber & Gasket Adhesive Features: Alight colored, high strength adhesive with a long tack rangeExcellent water, oil and grease resistanceBonds neoprene, natural, reclaim SB-R and butyl rubber to most substrates.Information.. |
|||
Brookfield Viscosity | 900 - 1200 cP | 900 - 1200 cP | LVF Sp #2 @30 rpm |
3M Scotch-Weld™ LO1000 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Brookfield Viscosity | 900 - 1300 cP | 900 - 1300 cP | RVT Model, Spindle #3 @ 20 rpm |
3M 32660 Heavy Duty Performance Coating - Part A 3M™ HD (Heavy Duty) Performance Coating is 100% solids elastomeric lining especially developed for high abrasion and tear resistance with thick build up characteristics. It has good durability and .. |
|||
Brookfield Viscosity | 900 cP @Temperature 25.0 °C |
900 cP @Temperature 77.0 °F |
|
Loctite® FLASHCURE™ 4303 Light Cure Instant Adhesive Cyanoacrylate Light Cure AdhesivesLoctite offers the most comprehensive line of adhesives and sealants available to the medical device industry. These USP class VI and/or ISO-10993 compliant product.. |