Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 525 - 1850 cP | 525 - 1850 cP | RVT Spindle 3 @ 20 rpm |
Palm Labs Adhesives TURBO SEAL SERIES 55 BROWN FINE THREADS THREAD SEALANT TURBO SEAL SERIES 55 is a high performance anaerobic thread sealant designed for the locking and sealing of metal threaded pipes and fittings. The product cures quickly in the absence of air between.. |
|||
Brookfield Viscosity | 525 cP | 525 cP | One Day Viscosity @ 6 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L100UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L100UF is a medium molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for th.. |
|||
Brookfield Viscosity | 525 cP | 525 cP | One Day Viscosity @ 6 rpmGeon® STP 1434 (with provided formulation); Internal Method |
PolyOne Geon™ 170 Series L120UF Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Ultrafine 170-L120UF is a high molecular weight, ultrafine particle size homopolymer dispersion resin. With the very fine particle size, it provides excellent casting characteristics for thin.. |