Physical Properties | Metric | English | Comments |
---|---|---|---|
Environmental Stress Crack Resistance | 6.0 hour | 6.0 hour | Cond. B, 10%; ASTM D1693 |
ExxonMobil HD 6704.18 Injection Molding Resin Product Description: HD 6704 is a narrow molecular weight hexane copolymer designed for outstanding balance of ESCR, Toughness and Stiffness properties. This resin is ideally suited for heavy-duty a.. |