Polymer Property : Oxygen Transmission Rate = 42.0 cc/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxygen Transmission Rate 652 cc/m²/day

@Temperature 23.0 °C
42.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Bicor™ 35MB666 OPP Film
Product Description: A is a biaxially oriented transparent polypropylene film, acrylic coated tow sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle E..
Oxygen Transmission Rate 652 cc/m²/day

@Temperature 23.0 °C
42.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 52MH647 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Ava..
Oxygen Transmission Rate 652 cc/m²/day

@Temperature 23.0 °C
42.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 52MH648 OPP Film
Product Description: A high speed super white opaque, modified higher density, biaxially oriented polypropylene film, coated one side acrylic, one side very low temperature seal (VLTS) coating. VLTS..
Oxygen Transmission Rate 652 cc/m²/day

@Temperature 23.0 °C
42.0 cc/100 in²/day

@Temperature 73.4 °F
0% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 52MHR647 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented PP film, humidity resistant acrylic coated two sides. This film is designed to wrap products with a high moistu..