Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 84.4 - 96.0 cc-mm/m²-24hr-atm | 214 - 244 cc-mil/100 in²-24hr-atm | 0% RH |
BiologiQ ESR-PE EcoStarch mLLDPE Blend Properties of 70% mLLDPE, 25% ESR, 5% additive blend - thin filmInformation provided by BiologiQ |