Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | Average value: 320 cc-mm/m²-24hr-atm Grade Count:25 |
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Fluorinated Ethylene Propylene (FEP), Molded/Extruded". Each property range of values reported is minimu.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NC-1500 FEP Coating Powder, White NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Up to a thickness of 100 microns per single coat.Proc.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NC-1539 FEP Coating Powder, Gray NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Multiple coats, up to 2,000 microns.Processing Method.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NC-1810 FEP Coating Powder, White NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.In.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON ND-1 FEP Dispersion, Translucent White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON ND-2 FEP Dispersion, Milky White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON ND-4 FEP Dispersion, Milky White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON ND-4GY FEP Dispersion, Gray NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0012 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0025 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0050 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0100 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0250 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-0500 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-1000 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-1500 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NF-2400 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-101 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: High speed wire and cable coatings.Information pro.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-120 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, cable jacketing, tubes.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-130 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Heavy wall wire insulation, cable jacketing, pipe, shrinka.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-21 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Suited to high speed extrusion .. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-30 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding.Applications: Heavy wall wire insulation, tubes, cable jacketing.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-40 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, transfer molding, compression molding.Applications: Films and s.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NC-1830 FEP Coating Powder, Gray NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Roto lining.In.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-20 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion molding, injection molding.Applications: Wire and cable coatings, films,.. |
|||
Oxygen Transmission | 320 cc-mm/m²-24hr-atm | 812 cc-mil/100 in²-24hr-atm | at 25°C |
Daikin NEOFLON NP-3000 FEP Pellets NEOFLON FEP molding materials are supplied as translucent white pellets for melt flow processes.Processing Methods: Extrusion.Applications: Ultra high speed wire and cable coatings.Information provi.. |