Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxygen Transmission | 0.00400 - 0.600 cc-mm/m²-24hr-atm | 0.0102 - 1.52 cc-mil/100 in²-24hr-atm | Average value: 0.0397 cc-mm/m²-24hr-atm Grade Count:28 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Oxygen Transmission | 0.00400 cc-mm/m²-24hr-atm | 0.0102 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
Oxygen Transmission | 0.00400 cc-mm/m²-24hr-atm | 0.0102 cc-mil/100 in²-24hr-atm | |
Dow Saran® 516 PVDC SARAN® 516 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, designed for sheet coextrusion and forming into rigid plastic barrier containers for food applications. It is supp.. |
|||
Oxygen Transmission | 0.00400 cc-mm/m²-24hr-atm | 0.0102 cc-mil/100 in²-24hr-atm | |
Dow Saran® 525 PVDC SARAN® 525 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, designed for sheet coextrusion and forming into rigid plastic barrier containers for food applications. It is supp.. |
|||
Oxygen Transmission | 0.00400 cc-mm/m²-24hr-atm | 0.0102 cc-mil/100 in²-24hr-atm | |
Dow Saran® 469 PVDC SARAN® 469 barrier polymer with a molecular weight of 83000, is a copolymer of vinylidene chloride and vinyl chloride, designed for cast film extrusion and coextrusion into barrier films used in fl.. |
|||
Oxygen Transmission | 0.00400 - 0.0470 cc-mm/m²-24hr-atm | 0.0102 - 0.119 cc-mil/100 in²-24hr-atm | Average value: 0.0219 cc-mm/m²-24hr-atm Grade Count:10 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |
|||
Oxygen Transmission | 0.00400 cc-mm/m²-24hr-atm | 0.0102 cc-mil/100 in²-24hr-atm | 20°C; 65% RH; Permeability increases significantly at higher moisture content. |
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ.. |