Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 42 - 56 g/10 min @Load 21.6 kg, Temperature 190 °C |
42 - 56 g/10 min @Load 47.6 lb, Temperature 374 °F |
Flow@21.6kg/Flow@2.16kg ratio > 70; ASTM D1283 |
NIZHNEKAMSKNEFTEKHIM PE 6753G (526H7) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 16 - 56 g/10 min @Load 21.6 kg, Temperature 190 °C |
16 - 56 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Kazanorgsintez PE2NT26-13 High Density Polyethylene Composite Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended for injection molding processin.. |