Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.25 - 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 - 0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6148C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.25 - 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 - 0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6152C (526H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.20 - 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6348K (486F3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.25 - 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 - 0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6948C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.20 - 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.20 - 0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 1532B (YD50G) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Melt Flow | 0.20 - 0.40 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.20 - 0.40 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 4132B (PA14D) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates very high long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 0.25 - 0.40 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 - 0.40 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1283/L |
NIZHNEKAMSKNEFTEKHIM PE 6949C (486H3) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Melt Flow | 0.20 - 0.40 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.20 - 0.40 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®. |