Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.2 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.2 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
SABIC P6006 Black High Density Polyethylene for Pipes Product Description: P6006 is a black compound high density (class MRS 8 - PE 80) polyethylene with bimodal distribution of molecular mass. It is specifically designed for Pressure Pipe applicatio.. |
|||
Melt Flow | 6.2 g/10 min @Load 2.16 kg, Temperature 260 °C |
6.2 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hybrid S466 ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Melt Flow | 6.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
6.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
LG Chemical 81HF SAN Resin High flow, Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include food receptacles, disposable li.. |
|||
Melt Flow | 6.2 g/10 min @Load 21.6 kg, Temperature 190 °C |
6.2 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 3 – 100S HM CRP 100 N High Density Polyethylene EX3-100S is a high density polyethylene with 1-Butene as co monomer. It is natural, outstanding ESCR, high impact strength, outstanding hydrostatic strength for PE 100 class.Applications: pipe extr.. |
|||
Melt Flow | 6.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
6.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Diamond Polymers ABS 3003MC Black 1722 Description: BlackInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 6.2 g/10 min @Load 3.80 kg, Temperature 300 °C |
6.2 g/10 min @Load 8.38 lb, Temperature 572 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY 627 PC/Polyester Alloy Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 6.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
6.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |