Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.9 g/10 min @Load 2.16 kg, Temperature 300 °C |
17.9 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP D451 PC (Asia Pacific) LNP* Thermocomp* D451 (or EXTC8141) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good duc.. |