Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® HPS2S PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML7678 PC 17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regio.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® VR2020 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-.. |
|||
Melt Flow | 17.5 g/10 min @Load 5.00 kg, Temperature 190 °C |
17.5 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
IRPC Polimaxx Polene R1760 High Density Polyethylene CHARACTERISTICS: HIGH IMPACT STRENGTH, EXCELLENT SURFACE APPEARANCE, GOOD RIGIDITY CONTAIN UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR CRATES, TRAYS, CASES, INDUSTRIAL PARTS, BINS, LAR.. |
|||
Melt Flow | 17.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
17.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ISO 1133 |
Total MDPE HR 515 Medium Density Polyethylene, Blown Film MDPE HR 515 is a medium density polyethylene produced with hexene as a co-monomer. It shows a broad molecular weight distribution ensuring outstanding processability.MDPE HR 515 is especially dedic.. |
|||
Melt Flow | 17.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
17.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 17.5 g/10 min @Load 1.00 kg, Temperature 235 °C |
17.5 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Diamond Polymers Softflex® 2701-1502R Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 17.5 g/10 min @Load 1.00 kg, Temperature 235 °C |
17.5 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Diamond Polymers Softflex® SF 5060 Overmold for Nylon Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 17.5 g/10 min @Load 1.00 kg, Temperature 235 °C |
17.5 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Diamond Polymers Softflex® SF 8900 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea.. |
|||
Melt Flow | 17.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
17.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |