Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 14.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
14.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
Procedure A Condition I; ASTM D1238 |
Network Polymers SAN 280 Water Clear Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc. |
|||
Melt Flow | 14.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers Softflex® 0921 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 14.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
14.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers SAN 280 Styrene Acrylonitrile, Transparent Engineering Thermoplastic Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |