Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.6 g/10 min @Load 5.00 kg |
1.6 g/10 min @Load 11.0 lb |
ASTM D 1238 |
Total Finathene® 7208 HDPE extrusion resin
(discontinued **) Applications: monofilament, slit tape, woven and knitted fabrics, specialty filmsInformation provided provided by Total Petrochemicals.Total Petrochemicals includes former Fina and Atofina plastics .. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Melt Flow | 1.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Melt Flow | 1.6 g/10 min @Load 5.00 kg, Temperature 190 °C |
1.6 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) EX 1 HF 7740F2 High Density Polyethylene EX1 (HF 7740F2) is high density polyethylene with Butene-1 as co monomer. It is a medium molecular mass with a narrow molar mass distribution.Application: stretched film tape used in manufacture o.. |
|||
Melt Flow | 1.6 g/10 min @Load 3.80 kg, Temperature 230 °C |
1.6 g/10 min @Load 8.38 lb, Temperature 446 °F |
ISO 1133 |
Styron EMERGEâ„¢ 5302 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5302 is a black, 20% glass-filled ABS which is suitable for use in a wide variety of internal structural component applications in the information technology market. Applications: .. |